Rock Wool

Features:

  • Small coefficient of heat conductivity and good capability of heating preservation, outstanding effect of energy-saving.
  • Excellent fireproof capability.
  • Excellent sound absorption and sound insulation capability.
  • Stable capability of chemistry may keep the long-term using.
  • No causticity effects the heat preservation materials.
  • Green building materials and no harm for body.
  • Broad using range.

Technical Performance:

Product Density (kg/m3) Thickness (mm) Length (mm) Width (mm)
Rock wool slab 60 50-80 1200 600
80 40-100 1000 630
100 30-100
120 40-80
150 40-60
180 40-60
Rock wool felt 80 50-100 3000 910
100 40-100
Rock wool pipe section 130 30-80 1000 18-350

Physical Performance:

Item Testing Result Standard
Density Tolerance (%) 8.3 ±15
Binder content (%) 2.9 ≤4.0
Working temperature (℃) 600 ≥600
Thermal conduct w/(m·k)(70±5℃) 0.04 ≤0.044
Combustion Non-combustible Non-combustible
Average Fiber Diameter (ūm) 5.7 ≤7.0
Slag Nodule Content (%) 4.2 ≤12.0
CIˉ 0.0058 ---

Thermal Insulation for Equipment and Pipes:

Types Properties Slab Faced Stitched Mat Pipe Section
Density  (kg/m3) 60-180 80-120 100-150
Thermal conduct equation  (w/m·k) 0.035+0.00018 tm 0.028+0.00023 tm 0.036+0.00015 tm
Working temperature ℃ 600 600 600
Application field Equipment with plane or big curve surface Equipment and big diameter pipes Pipes with small diameter

Chemical Composition:

Chemical Item Testing Result (%) Chemical Item Testing Result(%)
SiO2 42.21 MnO 0.31
Al2O3 11.88 Na2O 0.33
CaO 33.41 TiO2 0.81
MgO 9.24 K2O 0.65
Fe2O3 0.78 -

Physical-chemical Performance:

Item Testing Result Standard Result
Volume density(kg/m3) 148 ≤240
Averaged fiber diameter(mm) 4.8 ≤5.0
Water ratio(%) 0.03 ≤0.20
Organic matter content(%) 0.13 ≤0.30
Fiber strength(WT value mm) 65.3 ≥50
Acidity coefficient 1.27 ≥1.10
Grain size distribution(%)(>12mm) 95.3 ≥20.0
Slag particle content(%)(single diameter>0.5mm) 0.3 ≤2.0
Slag particle summation(%) 24.7 ≤25.0
Heat shrinkage temperature(℃) 702 ---
Combustibility Non-combustible Non-combustible

Thermal Coefficient:

Inspection Item Experiment Method W/(m·K) Measured Result
Average Temperature 50 ℃ GB/T10294-1988 0.042
Average Temperature 102 ℃ 0.046
Average Temperature 151℃ 0.053
Average Temperature 200℃ 0.058
Average Temperature 250 ℃ 0.064
Average Temperature 301 ℃ 0.073
Average Temperature 350 ℃ 0.08
Average Temperature 400 ℃ 0.086

Construction Requirement:

1.The consistency standards of the rock wool slab used 150kg per m3 above, and the intensity of pressure resistance of the slab of 150kg per m3 is equals to or more than 40KN per m2; and the intensity of pressure resistance of the slab of 180kg per m3 is equals to or more than 60KN per m2.

2.To achieve the best effect of heat preservation, double-layer rock wool slab need to lay in the break joint.

3.In the process of fixing the materials of heat preservation and waterproofing, or dealing with the gutter inlet, the special.

4.Fittings needed lo prevent water from contacting the rock wool slab directly.